Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp ZZ006 PPE+PS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* ZZ006 is a compound based on PPE+PS Blend resin containing Milled Glass.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.0 MPa
7830 psi
ASTM D 638
Flexural Strength 103 MPa
14900 psi
ASTM D 790
Flexural Modulus 4.45 GPa
645 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 123 °C

@Thickness 3.20 mm
253 °F

@Thickness 0.126 in
unannealed; ASTM D 648