Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183
Water Absorption 2.64 %

@Temperature 23.0 °C,
Time 86400 sec
2.64 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Moisture Absorption at Equilibrium 0.20 %
0.20 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0015 - 0.0025 cm/cm

@Time 86400 sec
0.0015 - 0.0025 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.010 - 0.012 cm/cm

@Time 86400 sec
0.010 - 0.012 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
5 mm/min; ISO 527
Tensile Modulus 9.40 GPa
1360 ksi
1 mm/min; ISO 527
Flexural Yield Strength 190 MPa
27600 psi
2 mm/min; ISO 178
Flexural Modulus 8.00 GPa
1160 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Hot Ball Pressure Test <= 240 °C
<= 464 °F
IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
UL RTI, Electrical 140 °C
284 °F
UL 746B
UL RTI, Mechanical with Impact 110 °C
230 °F
UL 746B
UL RTI, Mechanical without Impact 140 °C
284 °F
UL 746B
Flammability, UL94 V-0

@Thickness 0.400 mm
V-0

@Thickness 0.0157 in
UL 94
5VA

@Thickness 1.60 mm
5VA

@Thickness 0.0630 in
UL 94
Glow Wire Test 775 °C

@Thickness 0.400 mm
1430 °F

@Thickness 0.0157 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
775 °C

@Thickness 1.00 mm
1430 °F

@Thickness 0.0394 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
775 °C

@Thickness 1.50 mm
1430 °F

@Thickness 0.0591 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
825 °C

@Thickness 3.00 mm
1520 °F

@Thickness 0.118 in
Glow Wire Ignitability Temperature; IEC 60695-2-13
960 °C

@Thickness 0.400 mm
1760 °F

@Thickness 0.0157 in
Glow Wire Flammability Index; IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
ASTM D 257
Dielectric Strength 16.0 kV/mm

@Thickness 1.60 mm
406 kV/in

@Thickness 0.0630 in
in air; ASTM D 149
Comparative Tracking Index 600 V
600 V
IEC 60112
Hot Wire Ignition, HWI >= 120 sec
>= 120 sec
PLC code 0; UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
surface, PLC code 0; UL 746A