Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp PH0600A PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* PH0600A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 6.00 g/cc
0.217 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 62.0 MPa
8990 psi
ASTM D 638
Elongation at Break 3.6 %
3.6 %
ASTM D 638
Flexural Strength 96.0 MPa
13900 psi
ASTM D 790
Flexural Modulus 11.5 GPa
1670 ksi
ASTM D 790
Izod Impact, Notched 0.370 J/cm

@Temperature 23.0 °C
0.693 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 1.86 J/cm

@Temperature 23.0 °C
3.48 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812