SABIC Innovative Plastics LNP Thermocomp DX04021 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp DX04021 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* DX04021 is a compound based on Polycarbonate resin containing Stainless Steel. Added features include : FDA-Complaint Raw Materials, Metal Detectable.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 67.0 MPa
9720 psi
5 mm/min; ISO 527
Elongation at Break 5.2 %
5.2 %
5 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 103 MPa
14900 psi
2 mm/min; ISO 178
Flexural Modulus 2.70 GPa
392 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 130 °C
266 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af