SABIC Innovative Plastics LNP Thermocomp DFZ42P PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp DFZ42P PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0040 cm/cm

@Time 86400 sec
0.0040 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ASTM D 638
Elongation at Break 3.0 %
3.0 %
ASTM D 638
Tensile Modulus 5.71 GPa
828 ksi
50 mm/min; ASTM D 638
Flexural Strength 131 MPa
19000 psi
ASTM D 790
Flexural Modulus 5.57 GPa
808 ksi
ASTM D 790
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 5.73 J/cm

@Temperature 23.0 °C
10.7 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 131 °C

@Thickness 3.20 mm
268 °F

@Thickness 0.126 in
unannealed; ASTM D 648