SABIC Innovative Plastics LNP Thermocomp AF0029 ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp AF0029 ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* AF0029 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 64.0 MPa
9280 psi
5 mm/min; ISO 527
Elongation at Break 2.5 %
2.5 %
5 mm/min; ISO 527
Tensile Modulus 4.20 GPa
609 ksi
1 mm/min; ISO 527
Flexural Yield Strength 96.0 MPa
13900 psi
2 mm/min; ISO 178
Flexural Modulus 3.90 GPa
566 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94