SABIC Innovative Plastics LNP Thermocomp 4X08423

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp 4X08423.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* 4X08423 is a compound based on Perfluoroalkoxy Polymer (PFA) containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 2.20 g/cc
2.20 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 2.9 %
2.9 %
Type I, 5 mm/min; ASTM D 638
Tensile Modulus 5.13 GPa
744 ksi
50 mm/min; ASTM D 638
Flexural Yield Strength 45.0 MPa
6530 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2.88 GPa
418 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 1.24 J/cm

@Temperature 23.0 °C
2.32 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 3.17 J/cm

@Temperature 23.0 °C
5.94 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 169 °C

@Thickness 3.20 mm
336 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Users viewing this material also viewed the following: