Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF VC006 Super Tough PA 6/6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOTUF* VC006 is a compound based on Super Tough Nylon 6/6 resin containing Carbon Fiber. Added features of this material include: High Impact.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 157 MPa
22800 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Tensile Modulus 16.37 GPa
2374 ksi
50 mm/min; ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 14.55 GPa
2110 ksi
ASTM D790
Izod Impact, Notched 1.49 J/cm
2.79 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.43 J/cm
15.8 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C

@Thickness 3.20 mm
477 °F

@Thickness 0.126 in
unannealed; ASTM D648