SABIC Innovative Plastics LNP THERMOTUF RN001IX4 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF RN001IX4 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RN001X4 is a compound based on PA 66 resin containing MoS2. Added features include: Internally Lubricated, High Impact, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
5 mm/min; ISO 527
Elongation at Break 97 %
97 %
5 mm/min; ISO 527
Tensile Modulus 1.60 GPa
232 ksi
1 mm/min; ISO 527
Flexural Yield Strength 49.0 MPa
7110 psi
2 mm/min; ISO 178
Flexural Modulus 1.30 GPa
189 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 42.0 kJ/m²
20.0 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 116 µm/m-°C

@Temperature 23.0 - 60.0 °C
64.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 67.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
37.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 212 °C
414 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C
144 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af