SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF MX00619 PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermotuf* MX00619 is a compound based on Polypropylene resin containing Proprietary Filler(s).
Physical Properties Metric English Comments
Density 0.990 g/cc
0.0358 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Tensile Modulus 3.137 GPa
455.0 ksi
50 mm/min; ASTM D638
Flexural Strength 55.0 MPa
7980 psi
ASTM D790
Flexural Modulus 2.81 GPa
408 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.36 J/cm
6.29 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: