SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester, TP (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester, TP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Mineral, Glass Fiber. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.83 g/cc
0.0661 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 97.0 MPa
14100 psi
ASTM D638
Elongation at Break 1.5 %
1.5 %
ASTM D638
Tensile Modulus 13.92 GPa
2019 ksi
50 mm/min; ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 19.16 GPa
2779 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 209 °C

@Thickness 3.20 mm
408 °F

@Thickness 0.126 in
unannealed; ASTM D648