SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* WF-1004 is a compound based on Polybutylene Terephalate resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 109 MPa
15800 psi
5 mm/min; ISO 527
Elongation at Yield 3.3 %
3.3 %
5 mm/min; ISO 527
Tensile Modulus 6.60 GPa
957 ksi
1 mm/min; ISO 527
Flexural Yield Strength 169 MPa
24500 psi
2 mm/min; ISO 178
Flexural Modulus 6.00 GPa
870 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
18.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 113 µm/m-°C

@Temperature 23.0 - 60.0 °C
62.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 219 °C
426 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 192 °C
378 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af