Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP UF00AAS PPA (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphthalamide (PPA)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP UF00AAS PPA (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* UF00AAS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.63 g/cc
0.0589 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 234 MPa
33900 psi
5 mm/min; ISO 527
Elongation at Break 1.6 %
1.6 %
5 mm/min; ISO 527
Flexural Yield Strength 365 MPa
52900 psi
2 mm/min; ISO 178
Flexural Modulus 14.8 GPa
2150 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 269 °C
516 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: