Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RF0069XZ PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* RF0069XZ is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 165 MPa
23900 psi
ASTM D638
Elongation at Break 2.2 %
2.2 %
ASTM D638
Tensile Modulus 13.78 GPa
1999 ksi
50 mm/min; ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 11.72 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.94 J/cm
13.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 243 °C

@Thickness 3.20 mm
469 °F

@Thickness 0.126 in
unannealed; ASTM D648