Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RF0069SF PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* RF0069SF is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 174 MPa
25200 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Tensile Modulus 13.77 GPa
1997 ksi
50 mm/min; ASTM D638
Flexural Strength 241 MPa
35000 psi
ASTM D790
Flexural Modulus 11.43 GPa
1658 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.46 J/cm
12.1 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C

@Thickness 3.20 mm
239 °F

@Thickness 0.126 in
unannealed; ASTM D648