SABIC Innovative Plastics LNP THERMOCOMP RC004SXC PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP RC004SXC PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* RC004SXC is a compound based on PA66 resin containing Carbon Fiber. Added features include: Electrically Conductive, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
5 mm/min; ISO 527
Elongation at Break 3.0 %
3.0 %
5 mm/min; ISO 527
Flexural Strength 269 MPa
39000 psi
2 mm/min; ISO 178
Flexural Modulus 10.5 GPa
1520 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 17.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
9.44 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257