Material Notes:
LNP* THERMOCOMP* PX87791 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Moisture Absorption 0.900 %
0.900 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm

@Time 86400 sec
0.0060 - 0.0080 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 163 MPa
23600 psi
Type I, 5 mm/min; ASTM D638
Elongation at Break 2.5 %
2.5 %
Type I, 5 mm/min; ASTM D638
Flexural Strength 240 MPa
34800 psi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 1.12 J/cm
2.10 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.74 J/cm
14.5 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 213 °C

@Thickness 3.20 mm
415 °F

@Thickness 0.126 in
unannealed; ASTM D648