Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PFW53U PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PFW53U PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* PFW53U is a compound based on Nylon 6 resin containing Glass Fiber, Mineral. Added features of this material include: UV Stabilized.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 112 MPa
16200 psi
ISO 527
Elongation at Break 2.3 %
2.3 %
ISO 527
Tensile Modulus 8.50 GPa
1230 ksi
1 mm/min; ISO 527
Flexural Modulus 7.29 GPa
1060 ksi
ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
385 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved