Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* PF003 is a compound based on Nylon 6 resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 123 MPa
17800 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Tensile Modulus 6.35 GPa
921 ksi
50 mm/min; ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 5.60 GPa
812 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.30 J/cm
9.93 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D648