Material Notes:
LNP* THERMOCOMP* PF001S is a compound based on Nylon 6 resin containing 5% Glass Fiber. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 88.0 MPa
12800 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 3.97 GPa
576 ksi
50 mm/min; ASTM D638
Flexural Strength 131 MPa
19000 psi
ASTM D790
Flexural Modulus 3.57 GPa
518 ksi
ASTM D790
Izod Impact, Notched 0.420 J/cm
0.787 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 176 °C

@Thickness 3.20 mm
349 °F

@Thickness 0.126 in
unannealed; ASTM D648