Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PB006SXS PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* PB006SXS is a compound based on PA 6 resin containing Glass Bead. Added features include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Water Absorption 2.5 %

@Time 86400 sec
2.5 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
5 mm/min; ISO 527
Elongation at Yield 5.0 - 7.0 %
5.0 - 7.0 %
5 mm/min; ISO 527
Flexural Yield Strength 110 MPa
16000 psi
2 mm/min; ISO 178
Flexural Modulus 3.60 GPa
522 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af