Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP PB006EQ PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP *THERMOCOMP* PB006EQ is a compound based on PA 6 containing Glass Bead. Added features include Reduced Moisture.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.018 cm/cm
0.018 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
5 mm/min; ISO 527
Elongation at Break 10 %
10 %
5 mm/min; ISO 527
Flexural Yield Strength 56.0 MPa
8120 psi
2 mm/min; ISO 178
Flexural Modulus 2.40 GPa
348 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 109 µm/m-°C

@Temperature 23.0 - 60.0 °C
60.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 116 µm/m-°C

@Temperature 23.0 - 60.0 °C
64.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af