SABIC Innovative Plastics LNP THERMOCOMP MFB44S PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP MFB44S PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* MFB44S is a compound based on Polypropylene resin containing Glass Fiber, Glass Beads. Added features include; Heat Stabilized, Cu-Stabilized.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 50.0 MPa
7250 psi
5 mm/min; ISO 527
Elongation at Break >= 1.5 %
>= 1.5 %
5 mm/min; ISO 527
Tensile Modulus 5.60 GPa
812 ksi
1 mm/min; ISO 527
Flexural Yield Strength 65.0 MPa
9430 psi
2 mm/min; ISO 178
Flexural Modulus 4.20 GPa
609 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
257 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af