Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP KF006 POM (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* KF006 is a compound based on Acetal Copolymer resin containing Glass Fiber
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
ISO 1183
Water Absorption 0.40 %

@Time 86400 sec
0.40 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0080 - 0.011 cm/cm
0.0080 - 0.011 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 125 MPa
18100 psi
5 mm/min; ISO 527
Elongation at Break 2.9 %
2.9 %
5 mm/min; ISO 527
Tensile Modulus 9.20 GPa
1330 ksi
1 mm/min; ISO 527
Flexural Yield Strength 163 MPa
23600 psi
2 mm/min; ISO 178
Flexural Modulus 7.40 GPa
1070 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²
19.0 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 32.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
17.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 96.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
53.3 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 164 °C
327 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 161 °C
322 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af