Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP IF007 PA 6/12 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP IF007 PA 6/12 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* THERMOCOMP* IF007 is a compound based on Nylon 6/12 resin containing Glass Fiber.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 150 MPa
21800 psi
ASTM D638
Elongation at Yield 3.0 %
3.0 %
ASTM D638
Tensile Modulus 8.89 GPa
1290 ksi
50 mm/min; ASTM D638
Flexural Strength 227 MPa
32900 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 198 °C

@Thickness 3.20 mm
388 °F

@Thickness 0.126 in
unannealed; ASTM D648