SABIC Innovative Plastics LNP THERMOCOMP IB008 PA 6/12 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP IB008 PA 6/12 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* IB008 is a compound based on Nylon 6/12 resin containing Glass Bead.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.014 - 0.018 cm/cm
0.014 - 0.018 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 74.0 MPa
10700 psi
5 mm/min; ISO 527
Elongation at Break 3.6 %
3.6 %
5 mm/min; ISO 527
Flexural Strength 103 MPa
14900 psi
2 mm/min; ISO 178
Flexural Modulus 3.90 GPa
566 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 83.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.1 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 79.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
43.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
189 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af