Material Notes:
LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features include: Healthcare.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 166 MPa
24100 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Tensile Modulus 10.34 GPa
1500 ksi
50 mm/min; ASTM D638
Flexural Strength 262 MPa
38000 psi
ASTM D790
Flexural Modulus 10.34 GPa
1500 ksi
ASTM D790
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C

@Thickness 3.20 mm
399 °F

@Thickness 0.126 in
unannealed; ASTM D648