Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI (Asia Pacific)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP EC004XXC PEI (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* EC004XXC is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
1.34 g/cc
0.0484 lb/in³
ISO 1183
Moisture Absorption 0.200 %
0.200 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ASTM D955
0.0010 - 0.0030 cm/cm

@Time 86400 sec
0.0010 - 0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ASTM D955
0.0030 - 0.0050 cm/cm

@Time 86400 sec
0.0030 - 0.0050 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ASTM D638
175 MPa
25400 psi
ISO 527
Elongation at Break 2.0 %
2.0 %
ASTM D638
2.0 %
2.0 %
ISO 527
Tensile Modulus 14.5 GPa
2100 ksi
1 mm/min; ISO 527
Flexural Strength 250 MPa
36300 psi
ISO 178
259 MPa
37600 psi
ASTM D790
Flexural Modulus 12.0 GPa
1740 ksi
ISO 178
12.33 GPa
1788 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
10.0 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²
14.3 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 10.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
5.56 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
212 °C

@Thickness 3.20 mm
414 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.500 mm
V-0

@Thickness 0.0197 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D257