Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP THERMOCOMP DF004E PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DF004E PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* DF004E is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
ASTM D638
Elongation at Break 3.1 %
3.1 %
ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 6.27 GPa
909 ksi
ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C

@Thickness 3.20 mm
275 °F

@Thickness 0.126 in
unannealed; ASTM D648