SABIC Innovative Plastics LNP THERMOCOMP DF0029R PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP DF0029R PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* DF0029R is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Mold Release, Flame Retardant.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
5 mm/min; ISO 527
Elongation at Yield 3.9 %
3.9 %
5 mm/min; ISO 527
Tensile Modulus 3.80 GPa
551 ksi
1 mm/min; ISO 527
Flexural Yield Strength 120 MPa
17400 psi
2 mm/min; ISO 178
Flexural Modulus 3.30 GPa
479 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 9.00 kJ/m²
4.28 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
295 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 138 °C
280 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af