SABIC Innovative Plastics LNP THERMOCOMP AF001H ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOCOMP AF001H ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermocomp* AF001H is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 2.3 %
2.3 %
ASTM D638
Tensile Modulus 2.75 GPa
399 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 2.73 GPa
396 ksi
ASTM D790