Material Notes:
LNP* Stat-kon* ZE004 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D 792
1.17 g/cc
0.0423 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Time 86400 sec
0.0020 - 0.0040 in/in

@Time 24.0 hour
ASTM D 955
0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm

@Time 86400 sec
0.0040 - 0.0060 in/in

@Time 24.0 hour
ASTM D 955
0.0053 cm/cm

@Time 86400 sec
0.0053 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 103 MPa
14900 psi
ISO 527
104 MPa
15100 psi
ASTM D 638
Tensile Strength, Yield 54.0 MPa
7830 psi
ISO 527
80.0 MPa
11600 psi
ASTM D 638
Elongation at Break 0.50 %
0.50 %
ASTM D 638
0.90 %
0.90 %
ISO 527
Tensile Modulus 14.72 GPa
2135 ksi
1 mm/min; ISO 527
24.82 GPa
3600 ksi
50 mm/min; ASTM D 638
Flexural Strength 151 MPa
21900 psi
ISO 178
179 MPa
26000 psi
ASTM D 790
Flexural Modulus 12.7 GPa
1840 ksi
ISO 178
24.13 GPa
3500 ksi
ASTM D 790
Izod Impact, Notched 0.370 J/cm

@Temperature 23.0 °C
0.693 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 2.99 J/cm

@Temperature 23.0 °C
5.60 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 4.00 kJ/m²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
26.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
48.6 µm/m-°C

@Temperature -40.0 - 40.0 °C
27.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 36.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
37.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.6 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
139 °C

@Thickness 3.20 mm
282 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D 257