Material Notes:
LNP* Stat-kon* MD000IU is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact, UV Stabilized.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
0.980 g/cc
0.0354 lb/in³
ASTM D 792
Moisture Absorption at Equilibrium 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
50% RH; ASTM D 570
Linear Mold Shrinkage, Flow 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D 955
0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ASTM D 955
0.016 - 0.018 cm/cm

@Time 86400 sec
0.016 - 0.018 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D 638
17.0 MPa
2470 psi
ISO 527
Tensile Strength, Yield 18.0 MPa
2610 psi
ISO 527
21.0 MPa
3050 psi
ASTM D 638
Elongation at Break 133.8 %
133.8 %
ASTM D 638
Elongation at Yield 9.0 %
9.0 %
ASTM D 638
Tensile Modulus 0.480 GPa
69.6 ksi
50 mm/min; ASTM D 638
1.10 GPa
160 ksi
1 mm/min; ISO 527
Flexural Strength 20.0 MPa
2900 psi
ASTM D 790
27.0 MPa
3920 psi
ISO 178
Flexural Modulus 1.13 GPa
164 ksi
ASTM D 790
1.20 GPa
174 ksi
ISO 178
Izod Impact, Notched 8.33 J/cm

@Temperature 23.0 °C
15.6 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 15.48 J/cm

@Temperature 23.0 °C
29.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Izod Impact, Notched (ISO) 65.0 kJ/m²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 112 kJ/m²

@Temperature 23.0 °C
53.3 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Impact Test 31.0 J
22.9 ft-lb
Multiaxial Impact; ISO 6603
24.0 J

@Temperature 23.0 °C
17.7 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak; ASTM D 3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
101 µm/m-°C

@Temperature -40.0 - 40.0 °C
56.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 119 µm/m-°C

@Temperature -40.0 - 40.0 °C
66.1 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
119 µm/m-°C

@Temperature -40.0 - 40.0 °C
66.1 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C

@Thickness 3.20 mm
178 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C
133 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
52.0 °C

@Thickness 3.20 mm
126 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D 257