Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Stat-kon DX02731C PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Stat-kon DX02731C PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DX02731C is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 113 MPa
16400 psi
ASTM D 638
Elongation at Break 5.0 %
5.0 %
ASTM D 638
Flexural Strength 175 MPa
25400 psi
ASTM D 790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D 790
Izod Impact, Notched 0.640 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm

@Temperature 23.0 °C
10.0 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 3.20 mm
289 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Volume Resistivity 2.0 ohm-cm
2.0 ohm-cm
ASTM D 257
Surface Resistance 5.0 ohm
5.0 ohm
ASTM D 257