Material Notes:
LNP* Stat-kon* DEF13 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 118 MPa
17100 psi
ASTM D 638
Elongation at Break 4.0 %
4.0 %
ASTM D 638
Flexural Modulus 8.05 GPa
1170 ksi
ASTM D 790
Izod Impact, Notched 1.06 J/cm

@Temperature 23.0 °C
1.99 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 144 °C

@Thickness 3.20 mm
291 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Electrical Properties Metric English Comments
Surface Resistance 100 - 1.00e+6 ohm
100 - 1.00e+6 ohm
ASTM D 257