Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Stat-loy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-LOY PF303 PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-loy* PF303 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Antistat.
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.0 MPa
11900 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Tensile Modulus 5.04 GPa
731 ksi
50 mm/min; ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.08 GPa
592 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.53 J/cm
12.2 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 182 °C

@Thickness 3.20 mm
360 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved