Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Stat-loy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized.
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
ISO 1183
Water Absorption 8.5 %

@Time 86400 sec
8.5 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 43.0 MPa
6240 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
5 mm/min; ISO 527
Tensile Modulus 3.40 GPa
493 ksi
1 mm/min; ISO 527
Flexural Yield Strength 65.0 MPa
9430 psi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 48.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
26.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 124 µm/m-°C

@Temperature 23.0 - 60.0 °C
68.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 - 1.00e+12 ohm
1.00e+9 - 1.00e+12 ohm
ASTM D257
Copyright © lookpolymers.com All Rights Reserved