SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Stat-loy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-LOY A3000T ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-loy* A3000T is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: Antistat.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
5 mm/min; ISO 527
Elongation at Break >= 25 %
>= 25 %
5 mm/min; ISO 527
Tensile Modulus 1.30 GPa
189 ksi
1 mm/min; ISO 527
Flexural Strength 37.0 MPa
5370 psi
2 mm/min; ISO 178
Flexural Modulus 1.20 GPa
174 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 69.0 °C
156 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257