SABIC Innovative Plastics LNP STAT-KON PX08024 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON PX08024 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* PX08024 is a compound based on PA 6 resin containing Mineral. Added features include; Electrically Conductive, Easy Molding.
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.010 - 0.012 cm/cm
0.010 - 0.012 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 70.0 MPa
10200 psi
5 mm/min; ISO 527
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
5 mm/min; ISO 527
Tensile Modulus 4.80 GPa
696 ksi
1 mm/min; ISO 527
Flexural Yield Strength 105 MPa
15200 psi
2 mm/min; ISO 178
Flexural Modulus 4.20 GPa
609 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
16.7 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 1000 ohm - 1e+05
1000 ohm - 1e+05
ASTM D257