Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON OE008 PPS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP * Stat-kon* OE 008 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include: Electically Conductive.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 178 MPa
25800 psi
5 mm/min; ISO 527
Elongation at Break 0.70 %
0.70 %
5 mm/min; ISO 527
Tensile Modulus 30.3 GPa
4390 ksi
1 mm/min; ISO 527
Flexural Strength 251 MPa
36400 psi
2 mm/min; ISO 178
Flexural Yield Strength 253 MPa
36700 psi
2 mm/min; ISO 178
Flexural Modulus 25.3 GPa
3670 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 5.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
2.78 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 39.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
21.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257