SABIC Innovative Plastics LNP STAT-KON DX99620C PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DX99620C PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP STAT-KON* DX99620C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive.
Physical Properties Metric English Comments
Density 1.21 - 1.222 g/cc
0.0437 - 0.04415 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 4.13 GPa
599 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 5.05 J/cm
9.46 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °C

@Thickness 3.20 mm
133 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 100 - 1.00e+6 ohm-cm
100 - 1.00e+6 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257