Material Notes:
LNP* STAT-KON* DX95523C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 92.0 MPa
13300 psi
ASTM D638
Elongation at Break 1.4 %
1.4 %
ASTM D638
Tensile Modulus 15.85 GPa
2299 ksi
50 mm/min; ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 9.10 GPa
1320 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 140 °C

@Thickness 3.20 mm
284 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257