SABIC Innovative Plastics LNP Lubricomp DP003F PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Lubricomp DP003F PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D 792
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D 955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D 955
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D 638
Tensile Strength, Yield 42.0 MPa
6090 psi
ASTM D 638
Elongation at Break 15.3 %
15.3 %
ASTM D 638
Elongation at Yield 5.4 %
5.4 %
ASTM D 638
Flexural Strength 75.0 MPa
10900 psi
ASTM D 790
Flexural Modulus 2.15 GPa
312 ksi
ASTM D 790
Izod Impact, Notched 1.60 J/cm

@Temperature 23.0 °C
3.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 15.48 J/cm

@Temperature 23.0 °C
29.00 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812