Material Notes:
LNP LUBRILOY* UX99725 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ISO 1183
Water Absorption 0.46 %

@Time 86400 sec
0.46 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
SABIC Method
0.019 cm/cm

@Time 86400 sec
0.019 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.015 cm/cm

@Time 86400 sec
0.015 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 57.0 MPa
8270 psi
5 mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa
9140 psi
ISO 527
70.0 MPa
10200 psi
5 mm/min; ISO 527
Elongation at Yield 6.5 %
6.5 %
5 mm/min; ISO 527
Tensile Modulus 2.20 GPa
319 ksi
1 mm/min; ISO 527
Flexural Yield Strength 93.0 MPa
13500 psi
2 mm/min; ISO 178
Flexural Modulus 2.10 GPa
305 ksi
2 mm/min; ISO 178
2.36 GPa
342 ksi
ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 84.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
46.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af