SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Lubriloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubriloy* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 56.0 MPa
8120 psi
ASTM D638
Flexural Modulus 27.3 GPa
3960 ksi
ASTM D790
Izod Impact, Notched 0.740 J/cm
1.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 102 °C

@Thickness 3.20 mm
216 °F

@Thickness 0.126 in
unannealed; ASTM D648