Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP SP003 PA12 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP SP003 PA12 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* SP003 is a compound based on PA 12 resin containing PTFE/Silicone. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ISO 1183
Water Absorption 1.9 %

@Time 86400 sec
1.9 %

@Time 24.0 hour
ISO 62-1
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
50 mm/min; ISO 527
Tensile Strength, Yield 38.0 MPa
5510 psi
50 mm/min; ISO 527
Elongation at Break 35 %
35 %
50 mm/min; ISO 527
Elongation at Yield 2.9 %
2.9 %
50 mm/min; ISO 527
Tensile Modulus 2.00 GPa
290 ksi
1 mm/min; ISO 527
Flexural Strength 45.0 MPa
6530 psi
2 mm/min; ISO 178
Flexural Modulus 1.30 GPa
189 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 85.0 kJ/m²
40.4 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 130 µm/m-°C

@Temperature 23.0 - 60.0 °C
72.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 140 µm/m-°C

@Temperature 23.0 - 60.0 °C
77.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
268 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C
117 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af