SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RX05049 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* RX05049 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Proprietary Lubricant. Added features include; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0024 cm/cm
0.0024 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 173 MPa
25100 psi
5 mm/min; ISO 527
Elongation at Break 2.5 %
2.5 %
5 mm/min; ISO 527
3.3 %
3.3 %
Flexural Strain, break, 2 mm/min; ISO 178
Tensile Modulus 10.5 GPa
1520 ksi
1 mm/min; ISO 527
Flexural Strength 233 MPa
33800 psi
2 mm/min; ISO 178
Flexural Yield Strength 233 MPa
33800 psi
2 mm/min; ISO 178
Flexural Modulus 8.60 GPa
1250 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 22.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
12.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 77.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
42.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 248 °C
478 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af