Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RX01075 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RX01075 is a compound based on Nylon 66 resin containing PTFE, Mineral. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.64 g/cc
0.0592 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.0 MPa
8410 psi
5 mm/min; ISO 527
Elongation at Break 1.3 %
1.3 %
5 mm/min; ISO 527
Tensile Modulus 7.70 GPa
1120 ksi
1 mm/min; ISO 527
Flexural Yield Strength 88.0 MPa
12800 psi
2 mm/min; ISO 178
Flexural Modulus 6.70 GPa
972 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
47.2 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 217 °C
423 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Users viewing this material also viewed the following: