Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP QFL36 PA6.10 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP*Lubricomp* QFL36 is a compound based on PA 6/10 resin containing Glass Fiber, PTFE. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 123 MPa
17800 psi
5 mm/min; ISO 527
Elongation at Break 3.6 %
3.6 %
5 mm/min; ISO 527
Tensile Modulus 8.40 GPa
1220 ksi
1 mm/min; ISO 527
Flexural Yield Strength 180 MPa
26100 psi
2 mm/min; ISO 178
Flexural Modulus 6.90 GPa
1000 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
6.19 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 65.0 kJ/m²
30.9 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.70
0.70
ASTM D3702 Modified
Coefficient of Friction, Static 0.52
0.52
ASTM D3702 Modified
K (wear) Factor 30.2 x 10-8 mm³/N-M
15.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 27.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
15.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 107 µm/m-°C

@Temperature 23.0 - 60.0 °C
59.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 201 °C
394 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af