SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA 6/10 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 610
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA 6/10 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* QCL34 is a compound based on Nylon 6/10 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 17.16 GPa
2489 ksi
50 mm/min; ASTM D638
Flexural Strength 289 MPa
41900 psi
ASTM D790
Flexural Modulus 14.06 GPa
2039 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.14 J/cm
19.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 212 °C

@Thickness 3.20 mm
414 °F

@Thickness 0.126 in
unannealed; ASTM D648